Barrier Coat & Bottom Paint

Shel

Member
Member
Joined
Jun 14, 2004
RO Number
13987
Messages
421
Hi All,

I'm looking for some opinions and recomendations here.

I am thinking of using Interlux VC Tar2 epoxy barrier coat followed by Interlux VC 17 bottom paint.

I hear that the VC 17 is good for my Great Lakes area, and I know people who very pleased with it. It seems very easy to apply at the beginning of each season. Does anyone have any pros or cons of this bottom paint?

I have not heard of anyone having the VC Tar2 barrier, so I'm looking for any feedback on this.

Also, how do people get around the problem of coating the areas of the hull that are on blocks? Jacks? Can these areas be done after the rest of the hull is complete and dried?

Thanks for any info you can provide.
Shel
 
I stripped the bottom of my 1986 vessel in 2001. Since I didn't find any blisters, I simply coated with VC 17. TO date I have not had any blisters and have found the product works great on Lake Erie. I retouch every other year and repaint every other year ( the years that I don't retouch).
 
In 2002 I had the boat of my 1986 Silverton blasted and dried over the winter. In the spring the bottom was barrier coated and had VC-Offshore applied. Worked for about 3 seasons before having it touched up again.
 
I used the VC Tar and VC Offshore with good results in Lake Michigan. Nice thing about it is no build up and no sanding. Would still be using it but that was two boats ago.
 
Thanks for the feedback.

So there is no one that can help me with the problem of getting to the areas that are inaccessible due to the blocks? Was I right about using jacks? Can those areas be completed after the rest of the hull is done?

Thanks,
Shel
 
Shel
Our boat was on a trailer but the yard that did mine twice lifted it off and yes I could see where he touched up the sling marks. No problem doing that.
Good luck
Niles
 
If there are extra screw jacks use them to support the boat while you remove the jacks that are in the way.You will have to paint under the blocking when it is hoisted for launch.
 
There are 4-5 coats of barrier coat required (Like interlux 200OE).
After the last coat is completed and the touch-up-is started,
do you still apply 5 coats on the bare spots??

Is there still a perfect bond with the already 4-5 coats applied, after the touchup is completed??

Or-- should after every coat the boat be lifted and the the bare spots painted???
 
Don't know how large your boat is--with smaller boats, use bottle hyraulic jacks to lift either the bow or stern (put a 2 x 6 at least--and perhaps a 4 x 4" steel plate between the wood and the jack top. Then move the back blocks with two of the jacks. I have done boats up to 10,000 lbs with this technique--perhaps you could do larger--be sure that the blocking is adequate and use safety precautions of extra jack stands and blocks. I have some one following the jacks with blocks and wedges to avoid any surprises as I jack! Also best to use a long handle or air jack--that way you are not under the hull!

If the boat is to large for that, most yards include one lift when on blocks to reblock and allow you to paint the areas which were not done. Put wax paper under the areas allready coated. I also put carpet under the wax paper. I would put the full number of coats on the areas--you could use a faster cataylst and have a short pot life, since the areas are small, and probably do the coatings in a day or two. Be sure and wash off any amine blush between coatings.
 
John
Here's a trick to allow you 1 move of your supports.
1) Apply your barriers coats (all of them). Get as close to the blocked areas as you can.
2) Put on your antifouling coats, but avoid covering 3-5 inches of the barrier coat surrounding these blocked areas.
3) Move the blocks sufficiently that you have room to allow some antifouling overlap later.
4) Lightly sand the barrier coat as you prep the previously blocked areas. You'll want to feather the edges to minimize the appearance of an "ass-hole". (that's how an old body shop mentor described them to me years ago)
5) Apply your barriers coats overlapping the lightly sanded area (avoiding overlap on the antifouling).
6) Then apply antifouling, with some overlap over the existing antifouling. I used VC17M so I did not need to sand when overlapping the antifouling.

Worked well for me last winter.
 
Back