Sorry if this is in the wrong area..
I'll try and make this short and to the point. Last fall when I had my 25 Searay hauled and blocked at my house. After the stern was blocked he was working on the bow part (adjusting the bottle jack under the keel)so he could jack up the front and pull the trailer away. Well anyway the Bottle Jack top has a surface of about the size of a quarter. All of a sudden the boat bow slipped off the trailer and there was a crunch. The boat came down and put a hole in the bottom.
He finished blocking, left and came back and grinded/sanded the area and put something in the hole and glassed it. He said he would do a second application prior to me splashing it. When I asked him about it this year he said I'm good to go with out a second applicaction.
Does this sound right? Isn't there gellcoat needed after glassing? Any thought on this? I'm not in a hurry due to health reason I am not able to splash this year.
Thanks and I'm sorry this is so long.
Joe
I'll try and make this short and to the point. Last fall when I had my 25 Searay hauled and blocked at my house. After the stern was blocked he was working on the bow part (adjusting the bottle jack under the keel)so he could jack up the front and pull the trailer away. Well anyway the Bottle Jack top has a surface of about the size of a quarter. All of a sudden the boat bow slipped off the trailer and there was a crunch. The boat came down and put a hole in the bottom.
He finished blocking, left and came back and grinded/sanded the area and put something in the hole and glassed it. He said he would do a second application prior to me splashing it. When I asked him about it this year he said I'm good to go with out a second applicaction.
Does this sound right? Isn't there gellcoat needed after glassing? Any thought on this? I'm not in a hurry due to health reason I am not able to splash this year.
Thanks and I'm sorry this is so long.
Joe