Replacing bayliner floor

Remember that fiberglass has a 2% moisture absorption rate. Many people think fiberglass is impervious, but that is not true. Epoxy first, then glass is the way to go.

When I had water in my cabin, the only way to get everything dried out was to remove the carpet which was glued to the cabin sole. I replaced it with smaller sections of marine carpet which can be removed for cleaning or drying. I've had to remove it to dry out the cabin one other time. Thank goodness I did not glue the carpet pieces back into place!
 
I haven't used the 'new' pressure treated ply. Didn't know it existed. I've done a complete replacement of all wood between the transom and cuddy in my 24' searay. I used mostly exterior grade plywood sealed carefully and generously in epoxy. I used 24 gallons of epoxy(over $2k) to make sure everything was sealed and well bonded to the hull. As mentioned above, the deck is an important structural part of a boat.
 
I would use 3/4" Douglas Fir marine grade. Shock coating the raw wood with a mix of acetone and polyester resin is an often missed step that will seal the raw wood.
 
came from the factory with 1/2 with one layer of fiberglass on the top. No coating....dosnt even look like epoxy...on the bottom.

I found a place a half hour away with 1/2" marine grade fir for 63 bucks a sheet. JACKPOT!
I will use that and coat the bottom with epoxy and do a coat of epoxy on top, a layer of glass, and a 3rd coat of epoxy. Then finish it off with carpet.
 
one more question....how much epoxy do you think I need and how thick fiberglass should I use?
 
Up to you. I'm using 1 layer of 12oz biax on top and bottom. If you're just doing the top there's 24oz biax. Either way will use the same amount of resin. There's 4 to 10oz cloth but that wouldn't add much strenth. Whatever you use you will need more than a gallon. Also, coat the wood good before fiberglassing.
 
I wouldn't buy anymore than that. You can always get more but probably wont need it.
 
cms829, An alternative to the carpet you might want to consider is non-skid coating that is similar to painted on truck bed liner. It is available in a range of colors i.e. white, gray tan etc.. I believe it is a one part polyurethane base.
 
johnnyk, I think I saw a display at a show of the stuff you're talkin bout a few years ago.
Got any more info?
 
Try a search in "Boatfix". A quick look in my Cabelas '07 catalog shows "Tuff Coat", non-skid coating.
 
Ran a google search, found a few. 2 sounded good, my concern is how long they would hold up.
 
I've had good luck using chopped strand mat to glass in place new pieces of wood on my workboat, using PT wood and epoxy resin...

I'm in the process of redoing one of the integral trim tabs on my 1980 Carver. They are made of fiberglass with a 3/4" marine ply core, and one of them delaminated. So I plan to get some PT ply and epoxy it all in place. Since I still have the inner and outer skins of the trim tab I was also thinking of using 5200 to glue the whole thing together again, which may obviate the need for the epoxy, but I was worried about making sure there was a good even bond between the wood and the skin. So I have to do a little more research before starting this little project...
 
Pete,
I'm not at all convinced the 5200 is all it's cracked up to be. I used 5200 to seal the plywood top to the wood frame on my first hard top/cabin try. I used my finger to make a clean fillet from the excess 5200 that squeezed out of the joint. This is on the inside so it's out of UV or direct exposure to the weather. Within two years, the surface became gummy. There are a couple of other applications where it has happened, too. I also have 5200 applied where it's in good shape so I'm sure what the reason for the gummy surface or if it's like that inside the joint. It hasn't leaked, though.(over 15 years)

One thing, I would not think of using anything but epoxy to bond wood to fiberglass. Use epoxy straight to wet out the wood and fiberglass skin and use a thickened epoxy for filling and bonding.
 
I would use polyester resin for repairs on this model. The cost savings is significant, you can use more material. The rule as I have understood it is as follows, expoxy can fix polyester but polyester can't fix epoxy, so once you start using it you stay with it. I like layers of 24 oz woven, makybe two on top on one on the bottom, between each layer use random strand. Add tri-stitched glass running a few inches over both sides of the seam, this makes great reinforcment. Make sure use are using laminating resin for all but the last coat or two. Don't forget the prep... fair out, grinding, as large of surface as possiable; up to several inches, all locations where you go glass to "new" glass contact. I would use marine 3/4" doug fir plywood for strength on the a floor board. I have used plastic, like the moisture barrier under your home, to make a damm, drip pan or mold to assist against forces of gravity. Good luck.
 
mrknowitall,

What makes you say you would use polyesture on this model? From what Ive been reading, everything points to using epoxy resin. Obviously I would love to use a less expensive product but dont want to have any problems.

Im still toying around with the idea of using exterior grade plywood instead of marine grade...on coat of epoxy on the bottom, a base coat, a glass coat, and a final coat on the top.

Let me know what you think. Im doing this within the next two weeks if the weather cooperates.
 
Polyester resin is what the manufacture used to build the boat. I agree many positive things have been said about the expoxy, but I think it's over kill. I would not cut corners on the plywood quality and make sure it's douglas fir 3/4".
 
well...Im using exterior grade douglass fir. Just picked it up from a local lumber yard. Looks to be great hardly any voids visible. Just ordered 2 gallons of epoxy too. I'll coat the hell out of it and one layer of fiberglass 1.5 oz mat. So as soon as the glass and resin come....Im ready to go.
 
FYI I was a warranty manager for a Brunwick boat company in the 80's and 90's. I would be happy to give additional advise, but photo's would help. You need to make sure the repair gets tabbed in properly at the seams. Woven roving and triaxile fiberglass are a must or the repair will not last. I would make a non-skid surface on top of your repaired area by using glass beads.

Good luck
 
I've had consistently bad luck with polyester and I've glassed a lot of plywood. I use System 3 Epoxy, which is a fraction of the cost of West and is easier to mix. I'm glad the posters have convinced you to use glass top and bottom. Just make sure you pay attention to the edges of the plywood because that's where the moisture gets in over time, and plywood won't wick up much epoxy because of its consistency. I don't know where you are but wait for some warm weather. The cure time for epoxy goes up dramatically below about 60 degrees.
 